Monday
Jan112010
Process for Cleaning and Polishing Cobalt/Chromium
Minimum recommended process for electropolishing Cobalt/Chromium
This is effective ONLY with metal which does not contain colored oxide:
Step |
Process Line / Description |
---|---|
1. |
Clean in MicroClean Ti™ (RDZ-1849) (Time and temperature to be determined, no such thing as “too much”) |
2. |
Water Rinse |
3. |
Alcohol Rinse |
4. |
ElectroPolish Ti2 (RDZ-1676), 300+ Amps/ft2, up to 10 minutes |
This process is effective for metal which has colored oxide:
Step |
Process Line |
Concentration & Temperature |
Equipment Required |
Ventilation Requirements |
---|---|---|---|---|
1. |
Pre-Clean in MicroClean Ti™ (RDZ-1849) |
100% 50°+ C |
SS labware PP or PVC |
Not Required |
2. |
Rinse in tap water |
|||
3. |
50% Part A 50% Part B 80°–100° C 4-24 hours |
Pyrex or SS |
Not Required |
|
4. |
Rinse in tap water |
Room Temperature |
||
5. |
100% Room Temp 60 Seconds |
Glass or Plastic |
Recommended |
|
6. |
Rinse in tap water |
|||
7. |
Rinse in dry alcohol |
??? |
||
8. |
100% Room Temperature |
SS |
Required |
|
9. |
Rinse in water |
tagged processes in Medical Equipment Industry